ZHANG Ya-hui, YOU Jia, YANG Chan, et al. Durability of Wood Scrimber for Outdoor Use by Accelerated Aging Tests. [J]. China Wood Industry 32(1):33-35(2018)
ZHANG Ya-hui, YOU Jia, YANG Chan, et al. Durability of Wood Scrimber for Outdoor Use by Accelerated Aging Tests. [J]. China Wood Industry 32(1):33-35(2018) DOI: 10.19455/j.mcgy.20180108.
Durability of Wood Scrimber for Outdoor Use by Accelerated Aging Tests
Poplar and larch veneers were used to manufacture wood scrimber samples, respectively.Mechanical properties and dimensional stability of the samples were evaluated by two accelerated aging test standards, like ASTM D 1037-2006 a "Standard Test Methods for Evaluating Properties of Wood-Base Fiber and Particle Panel Materials" and GB/T 17657-2013 "Test Methods for Evaluating the Properties of Wood-based Panels and Surface Decorated Wood-based Panels".Testing results showed that modulus of rupture(MOR), modulus of elasticity(MOE), compression strength(CS), shear strength(SS) and dimensional stability of the samples were all declined, but the MOR,MOE and dimensional stability could still meet the requirements of the Chinese Standard GB/T20241-2006 for structural material and GB/T 30364-2013 for outdoor floor use. Finally, it was found that test conditions of GB/T 17657-2013 were stricter than that of ASTM D 1037-2006 a.