Enclosing a Steam Injection Press for Manufacturing Low Density Fiberboard
This study focused on enclosing a steam-injection press,to eliminate any steam leakage,to produce low density(0.3 g/cm3) fiberboard.After reviewing this technology from previous studies,the authors designed an orthogonal experiment to optimize the process parameters for making low density fiberboard.The results indicated that when 10% resin content,160 ℃ pressing temperature,10 s steam injection time,and 10 s/mm pressing time were used,the properties of fiberboards met the requirements of national standard GB/T 17567-1999.
关键词
闭式喷蒸热压软质纤维板热压工艺
Keywords
enclosingsteam-injection pressinglow density fiberboardhot-pressing technology