Study on Mixing Conditions for Polypropylene and Wood Fiber
- Issue 1, Pages: 27-29(2005)
DOI: 10.19455/j.mcgy.2005.01.008
扫 描 看 全 文

1. College of Wood Science and Technology, Nanjing Forestry University
扫 描 看 全 文
[1]张立芳.聚丙烯与木纤维的复合研究[J].木材工业,2005(01):27-29.
ZHANG Li-fang. Study on Mixing Conditions for Polypropylene and Wood Fiber. [J]. China Wood Industry (1):27-29(2005)
通过检测以木纤维和聚丙烯为原料制造的木塑复合材料的抗拉强度,研究了木纤维和聚丙烯的复合性能,并分析了木纤维与聚丙烯的质量比、马来酸酐改性聚丙烯及偶联剂对复合材料抗拉强度的影响。试验结果表明,当聚丙烯与木纤维的混合比为10∶3、偶联剂加入量约为聚丙烯质量的3%~5%时,木塑复合材料的抗拉性能最佳。
The composites investigated in this paper were made from wood fibers either with (polypropylene) only, or with polypropylene modified with maleic anhydride or alternatively coupled with a silane agent. The adhesion between wood fiber and polypropylene was evaluated (through) (testing) the tensile strength of the composite. An analysis was made on how the tensile strength was influenced by the ratio of wood fiber to polypropylene, as well as the effect of the addition of maleic anhydride and the silane coupling agent to polypropylene. It was found that when the polypropylene and wood fiber was mixed at 10∶3 and 3%~5% coupling agent was added to polypropylene, the wood-polypropylene composite showed the best tensile strength.
聚丙烯木纤维抗拉强度
PolypropyleneWood fibersTensile strength