Study on Performance Improvement of Wood Preservative CCB
- Issue 3, (1995)
DOI: 10.19455/j.mcgy.1995.03.004
扫 描 看 全 文

1. Nanjing Forestry University
扫 描 看 全 文
[1]尤纪雪,宋桢.CCB木材防腐剂性能改善的研究[J].木材工业,1995(03):13-15.
Study on Performance Improvement of Wood Preservative CCB. [J]. China Wood Industry (3).(1995)
CCB是一种性能优良的木材防腐剂,但它的抗流失性能不如CCA,由于它是水溶性防腐剂,故处理后木材的尺寸亦不稳定。本研究采用在防腐剂中添加聚合物或树脂的方法来提高CCB的抗流失性能,使CCB处理材的尺寸稳定性大大提高。研究结果表明,在CCB中添加少量聚乙烯醇缩醛树脂后,铜、铬、硼的流失与不加树脂相比分别减少57.63,78.53和96,46%;木材湿胀性在弦向减少91.97%、径向减少88.34%、体积减少84,20%;处理材的抗腐力也明显提高。
CCB is an excellent wood preservative. But its anti-leaching is not as good as thatof CCA. Because CCB is a water soluble preservative,the dimension of wood will be changedafter treatment with CCB. This study attempts to improve the anti-leaching of CCB and di-mensional stability of the treated wood by means of adding some polymer or resin into thepreservative. The results showed that after a small amount of polyvinyl acetals resin wasadded into CCB the leaching of copper,chromium,boron decreaced 57.63,78.53 and 96.4%respectively,the tangential,radical and volumetric wet-swelling rates decreased 91.97,88.34,84.20%,The decay resistance of treated wood was improved distinctly.
CCB木材防腐剂聚乙二醇聚乙烯醇缩醛树脂抗流失性木材湿胀性
Wood preservative CCBPolyethylene glocolsPolyvinyl acetals resinAnti-leachingWet-swelling rates